CERAMIC MAGNETS
Tolerances

For as pressed material, tolerance on the thickness (direction of magnetization) is ± .005. Other dimensions are ± 2.5% or ± .010, whichever is greater. According to IMA standards, visual imperfections such as hairline cracks, porosity and minor chips are commonly found in sintered metallic magnets. A chipped edge is considered acceptable if no more than 10% of the surface is missing. Cracks are acceptable as long as they do not extend across more than 50% of pole surface.

Magnetizing and Handling

Ceramic magnet material is extremely brittle and can chip or break if dropped on a hard surface, or if allowed to “jump at” an attracting object. Handle with care. The weakest grade of ceramic material is grade 1, which is typically non-oriented. Grades 5 and 8 are oriented ceramic material. Grade 8 is the strongest ceramic magnet material available (Refer to properties chart below). When making magnetic assemblies with ceramic, it is typically easier for production purposes to magnetize the product after assembly.

Machining

Since ceramic material is so brittle, it requires special machining techniques and equipment. We are fully equipped to cut and grind ceramic material to your specifications.


Copyright 1998-2010 Master Magnetics, Inc. All rights reserved.
Colorado • California • Florida • Ohio | Your Best Source in the Magnetic Field |
Site Map